[1]李迎珠,张 勤,李文杰,等.氯盐环境下钢筋连接件受拉破坏特性研究[J].西安建筑科技大学学报(自然科学版),2023,55(04):546-554.[doi:10.15986/j.1006-7930.2023.04.009 ]
 LI Yingzhu,ZHANG Qin,LI Wenjie,et al.Investigation on tensile failure characteristics of steel connectors under corrosive environment[J].J. Xi'an Univ. of Arch. & Tech.(Natural Science Edition),2023,55(04):546-554.[doi:10.15986/j.1006-7930.2023.04.009 ]
点击复制

氯盐环境下钢筋连接件受拉破坏特性研究()
分享到:

西安建筑科技大学学报(自然科学版)[ISSN:1006-7930/CN:61-1295/TU]

卷:
55
期数:
2023年04期
页码:
546-554
栏目:
出版日期:
2023-10-26

文章信息/Info

Title:
Investigation on tensile failure characteristics of steel connectors under corrosive environment
文章编号:
1006-7930(2023)04-0546-09
作者:
李迎珠1张 勤1李文杰2杨翘楚1李 佳3贡金鑫3
(1.河海大学 土木与交通学院,江苏 南京 210024; 2.中国交通建设集团有限公司,北京 100088; 3.大连理工大学 建设工程学部,辽宁 大连 116024)
Author(s):
LI Yingzhu1 ZHANG Qin1 LI Wenjie2 YANG Qiaochu1 LI Jia3 GONG Jinxin3
(1.College of Civil and Transportation Engineering, Hohai University, Nanjing 210098, China; 2.China Communications Construction, Beijing 100088, China; 3.Faculty of Infrastructure Engineering, Dalian University of Technology, Dalian 116024, China)
关键词:
钢筋连接件 腐蚀 拉伸性能 破坏形态 强度
Keywords:
steel connector corrosion tensile property tensile failure characteristic strength
分类号:
TU375.3
DOI:
10.15986/j.1006-7930.2023.04.009
文献标志码:
A
摘要:
为研究不同钢筋连接件在腐蚀环境下的拉伸性能和破坏特性,对不同直径及腐蚀程度的双面电弧焊、套筒冷挤压、镦粗直螺纹和灌浆套筒四种钢筋连接件分别进行电化学腐蚀试验和拉伸性能试验,研究钢筋直径、腐蚀程度及连接方式对钢筋连接件受拉破坏特性的影响,并建立不同腐蚀程度下钢筋连接件拉伸破坏强度计算模型.结果表明:腐蚀环境下钢筋连接件的抗拉性能明显下降,且受钢筋直径和腐蚀程度的影响明显; 相同腐蚀程度下,灌浆套筒连接件的拉伸性能相较于其他连接方式的钢筋连接件更为稳定,当理论腐蚀率为20%时,其拉伸荷载-位移曲线仍有明显的屈服平台,破坏强度可达到未腐蚀试件的95%; 所建立的拉伸破坏强度计算模型可用于腐蚀环境下钢筋连接件抗拉性能评估和破坏强度预测.
Abstract:
In order to study the tensile properties and the failure pattern of different steel connectors in the corrosive environment, electrochemical corrosion test and tensile test for four kinds of steel connectors such as double-sided arc welding, cold extrusion sleeve, upsetting straight thread sleeve and grouting sleeve were carried out respectively. The effects of steel bar diameter, corrosion degree and connection mode on the tensile failure characteristics of steel connectors were studied, and the calculation model of tensile failure strength of steel connectors under different corrosion degrees was established. The results show that the tensile properties of the steel connectors degenerate obviously under the corrosion environment, and the connection properties of the connectors are more obviously affected by the corrosion levels and the diameters. With the same corrosion levels, the tensile properties of the grouting sleeve connectors are more stable than that of the other three kinds of connectors. Also, the load-displacement curves of the grouting sleeve connectors still keep an obvious yield plateau even under the corrosion level with 20% theoretical corrosion ratio, and the corresponding failure strength can still reach 95% of that of the uncorroded specimen. Furthermore, the proposed calculation model of the tensile failure strength of corroded steel connectors can be used to evaluate the tensile properties and predict the failure strength of steel connectors in the corrosive environment.

参考文献/References:

[1]王茹, 王希彤, 吕伯阳, 等. 灌浆套筒连接缺陷对装配式混凝土柱抗震性能的影响[J]. 武汉大学学报(工学版), 2023,56(6): 685-693.
WANG Ru, WANG Xitong, LV Boyang, et al. Study on the effect of the grouting sleeve splicing defects on the seismic behavior of precast concrete columns.[J]. Engineering Journal of Wuhan University, 2023,56(6):685-693.
[2]中华人民共和国住房和城乡建设部. 混凝土结构设计规范: GB 50010—2010[S]. 北京:中国建筑工业出版社, 2011.
Ministry of Housing and Urban-Rural Development of the People's Republic of China. Code for design of concrete structures: GB 50010—2010[S]. Bei Jing: China Building Industry Press, 2011.
[3]朱东烽, 练水泉, 张伟生, 等. 新型钢筋套筒挤压连接技术在装配式建筑的应用研究[J]. 建筑结构, 2020,50(22): 51-56, 76.
ZHU Dongfeng, LIAN Shuiquan, ZHANG Weisheng, et al. Research on the application of new steel-reinforced sleeve extrusion connection technology in assembled buildings[J]. Building Structure, 2020, 50(22): 51-56, 76.
[4]中华人民共和国住房和城乡建设部. 装配式混凝土建筑技术标准: GB/T51231—2016[S].北京:中国建筑工业出版社,2017.
Ministry of Housing and Urban-Rural Development of the People's Republic of China. Technical standard for prefabricated concrete construction: GB/T51231—2016[S]. Beijing: China Building Industry Press, 2017.
[5]李佳, 张勤, 贡金鑫, 等. 钢筋连接区锈蚀后的抗拉性能及破坏形态试验研究[J]. 建筑结构, 2020,50(22):83-88.
LI Jia, ZHANG Qin, GONG Jinxin, et al. Experimental study on tensile properties and failure patterns of corroded steel bars joint region[J]. Building Structure, 2020, 50(22): 83-88.
[6]SUN W W, FENG W. Numerical investigation of the effects of connection rotational stiffness on block shear capacity of coped beams with a welded end connection[J]. International Journal of Steel Structures. 2011,11(3): 325-333.
[7]OSTERTAG C P, Microstructure characterization of fractured steel beam-to-column connections[J]. Journal of Materials Science, 1999, 34(16): 3883-3891.
[8]黄远, 朱正庚, 黄登, 等. 钢筋半套筒灌浆连接的静力拉抻试验研究[J]. 华南理工大学学报(自然科学版), 2016,44(2):26-32.
HUANG Yuan, ZHU Zhenggeng, HUANG Deng, et al. Investigation into Half Grout Sleeve Splicing for Rebars via Static Tensile Test[J]. Journal of South China University of Technology(Natural Science Edition), 2016,44(2):26-32.
[9]郑清林, 王霓, 陶里, 等. 套筒灌浆缺陷对装配式混凝土柱抗震性能影响的试验研究[J]. 土木工程学报, 2018,51(5):75-83.
HENG Qinglin, WANG Ni, TAO Li, et al. Experimental study on effects of grout defects on seismic performance of assembled concrete columns[J]. China Civil Engineering Journal, 2018, 51(5):75-83.
[10]吴小宝, 林峰, 王涛. 龄期和钢筋种类对钢筋套筒灌浆连接受力性能影响的试验研究[J]. 建筑结构, 2013,43(14):77-82.
WU Xiaobao, LIN Feng, WANG Tao. Experimental research on effects of grout age and types of steel bars on mechanical behavior of grout sleeve splicing for reinforcing bars[J]. Building Structure, 2013,43(14): 77-82.
[11]徐港, 王青, 卫军, 等. 锈蚀钢筋搭接性能试验研究[J]. 武汉大学学报(工学版), 2011,44(6):726-730.
XU Gang, WANG Qing, WEI Jun, et al. Experimental study of behavior of lap splice of corrosive reinforcing bars in concrete[J]. Engineering Journal of Wuhan University, 2011,44(6):726-730.
[12]APOSTOLOPOULOS C A, MICHALOPOULOS D, DIMITROV L. The impact of corrosion on the mechanical behavior of welded splices of reinforcing steel S400 and B500c[J]. Journal of Materials Engineering and Performance, 2008,17(1):70-79.
[13]TANG L Y, XIAO Q H, ZHANG S Y. Corrosion properties of rebar welded joints[J]. Applied Mechanics and Materials, 2012,166-169:1981-1986.
[14]YOSUKE A, SHINICHI M, KYOJI N, et al. Influence of Chloride Ion Concentration and Sress on Steel Corrosion in Cement Paste Grout[J]. Doboku Gakkai Ronbunshuu E, 2009,65(1):103-117.
[15]中华人民共和国住房和城乡建设部. 钢筋焊接及验收规程: JGJ 18—2012[S]. 北京:中国建筑工业出版社, 2012.
Ministry of Housing and Urban-Rural Development of the People's Republic of China. Steel welding and acceptance procedures: JGJ 18—2012[S]. Bei Jing: China Building Industry Press, 2012.
[16]中华人民共和国住房和城乡建设部. 钢筋机械连接技术规程: JGJ 107—2016[S]. 北京:中国建筑工业出版社,2016.
Ministry of Housing and Urban-Rural Development of the People's Republic of China. Technical specification for mechanical connection of rebar: JGJ 107—2016[S]. Beijing: China Building Industry Press, 2016.
[17]金南国, 何家豪, 付传清, 等. 钢筋加速非均匀锈蚀试验方法和锈蚀形态研究[J]. 浙江大学学报(工学版), 2020,54(3):483-490.
Jin Nanguo, He Jiahao, Fu Chuanqing, et al. Study on experimental method and morphology of accelerated non-uniform corrosion of steel bars[J]. Journal of Zhejiang University(Engineering Science), 2020, 54(3): 483-490.

相似文献/References:

[1]张广平,杨飞龙,张 轶,等.光伏支架中螺栓连接和拉铆连接腐蚀前后抗剪性能对比试验研究[J].西安建筑科技大学学报(自然科学版),2022,54(04):569.[doi:10.15986/j.1006-7930.2022.04.012]
 ZHANG Guangping,YANG Feilong,ZHANG Yi,et al.Comparative experimental study on shear performance of bolt connection and riveting connection in photovoltaic bracket before and after corrosion[J].J. Xi'an Univ. of Arch. & Tech.(Natural Science Edition),2022,54(04):569.[doi:10.15986/j.1006-7930.2022.04.012]

备注/Memo

备注/Memo:
收稿日期:2022-11-11修回日期:2023-07-17
基金项目:国家自然科学基金资助项目(52278496、51978125),江苏省自然科学基金资助项目(BK20211206)
第一作者:李迎珠(1997—),女,工学硕士.主要从事钢筋混凝土耐久性等研究.E-mail:hhulizzyli@163.com
通信作者:张 勤(1983—),男,工学博士(博士后),副教授.主要从事钢筋混凝土结构抗震及耐久性等研究.E-mail:zhangqin8190@163.com
更新日期/Last Update: 2023-08-28