[1]马立建,刘民生.彩色显像管成型锥显微结构及抗侵蚀性[J].西安建筑科技大学学报:自然科学版,2011,43(01):143-0146.[doi:DOI:10.15986/j.1006-7930.2011.01.012]
 MA Li-jian LIU Min-sheng.study on microstructure and glass melt corrosion resistance of color picture tube forming cone[J].J.Xi’an Univ. of Arch. & Tech.:Natural Science Edition,2011,43(01):143-0146.[doi:DOI:10.15986/j.1006-7930.2011.01.012]
点击复制

彩色显像管成型锥显微结构及抗侵蚀性()
分享到:

西安建筑科技大学学报:自然科学版[ISSN:1006-7930/CN:61-1295/TU]

卷:
43
期数:
2011年01期
页码:
143-0146
栏目:
出版日期:
2011-02-28

文章信息/Info

Title:
study on microstructure and glass melt corrosion resistance of color picture tube forming cone
文章编号:
1006-7930(2011)01-0143-04
作者:
马立建 刘民生
(1.西安建筑科技学,陕西 西安 710055; 2、西部建筑科技国家重点实验室(筹),陕西 西安 710055
Author(s):
MA Li-jian12 LIU Min-sheng12
(1School of Materials Science and Engineering., Xian University. of Architecture &Technology. Xian 710055, China 2State Key Laboratory of Architecture Science and Technology in West China( XAUAT), Xian 710055, China)
关键词:
显微结构、成型锥、彩色显像管、侵蚀、玻璃熔体、莫来石
Keywords:
microstructure forming cone color picture tube corrosion glass melt mullite
分类号:
TQ154.1
DOI:
DOI:10.15986/j.1006-7930.2011.01.012
文献标志码:
A
摘要:
采用光学显微镜(DM)、x-射线衍射(XRD)及拉曼光谱研究了彩色显像管成型锥的显微结构及其抗玻
璃液的侵蚀性.结果分析表明:该成型锥属多相非均一结构,有利于提高材料的高温力学性能,在高温下成型
锥中的莫来石相与显像管玻璃熔体中的PbO、SrO、K2O、Na2O等组分反应生成物,在成型锥的使用温度下多
为高粘度,高温稳定相,同时由于“饱和状态”降低了玻璃熔体对成型锥的进一步侵蚀.
Abstract:
The microstructure and glass melt corrosion resistance of color picture tube forming cone were investigated by means of optical microscope, x-ray diffraction and Raman spectrometer. The experimental results indicate that: this forming cone has multi-phase heterogeneously structure, which helps improve the high temperature mechanical properties, at high temperature, the productions of reaction between mullite which has existed in forming cone and PbO、SrO、K2O、Na2O which came from glass melt are with high viscos, and with high temperature stable phase. Meanwhile the hyper saturated state is of benefit to glass melt corrosion resistance of forming cone

参考文献/References:

[1] 吉木文平非金属矿物工学[M]. 张绥庆译北京:出版社[M]. ZHANG Sui-qing translated. Beijing: Science Press 1962.
[2] 翁润生,工业岩石学[M]. 北京:出版社[M]. Beijing: China University of Geosciences Press 1990.
[3] LEVIN E. M., ROBBINS C. R., and MCMURDIE H. F., Phase Diagrams for Ceramists, American Ceramic Society, 1964.
[4] HEIJMAN M J G W, BENES N E, TEN E J E, Quantitative analysis of micro-structural homogeneity of zirconia - toughened alumina composite[J]. Materials Research Bulletin , 2002, 37:141 – 149.
[5] 李余增,热分析[M]. 北京:出版社[M]. Beijing: Tsinghua University Press 1987.
[6] 尹洪峰、高魁、任耘,等 硅酸盐通报[J]. 莫来石—钛酸铝高温窑具的研制 2008,27(4)808—811.
YIN Hong-feng,GAO Kui,REN Yun,et al.,Development of Mullite—Aluminium Titanate High Temperature
Kiln Furniture[J].Bulletin of the Chinese Ceramic Society,2008,27(4):808-811.

备注/Memo

备注/Memo:
收稿日期:2010-02-03  修改稿日期:2010-12-24
基金项目:陕西省教育厅重点产业化培育资助项目(04JC17)
作者简介:马立建(1973-),男,河南原阳人,博士生,讲师,主要从事无机非金属材料的教学和研究工作.
更新日期/Last Update: 2015-11-01